Chemical Properties | ||||||||
---|---|---|---|---|---|---|---|---|
C | Si | Mn | P | S | Cr | Mo | V | Al |
0.36-0.47 | 0.15-0.35 | 0.45-0.70 | 0.035 Max | 0.040 Max | 0.80-1.15 | 0.50-0.65 | 0.25-0.35 | 0.015 Max |
Mechanical Properties | ||||||
---|---|---|---|---|---|---|
Proof Load Using Threaded Mandrel- METRIC (kN) | ||||||
TYPE | M6 | M8 | M10 | |||
HEAVY HEX | 29.2 | 44.1 | 69.9 | |||
HEX | 20.8 | 37.9 | 60 | |||
TYPE | M20 | M22 | M24 | |||
HEAVY HEX | 295.2 | 365.1 | 425.4 | |||
HEX | 253.6 | 313.6 | 365.4 | |||
Hardness | ||
---|---|---|
BHN | HRB | |
Min | ||
248-352 | - | |
Heat Treatment | ||||||
---|---|---|---|---|---|---|
Quenched & Tempered@650°C. | ||||||